Which casting defect occur due to excess moisture content in moulding sand ?

This question was previously asked in
MP Sub Engg Official Mechanical Paper (Held on 9 July 2017 - Shift 2)
View all MP Vyapam Sub Engineer Papers >
  1. Porosity
  2. Shrinkage
  3. Blow holes
  4. Inclusions

Answer (Detailed Solution Below)

Option 3 : Blow holes
Free
Building Materials for All AE/JE Civil Exams Mock Test
20 Qs. 20 Marks 20 Mins

Detailed Solution

Download Solution PDF

Explanation:

Some of the defects encountered in casting are mentioned below.

Blow holes:

  • Blow holes, gas holes, or gas cavities are well-rounded cavities having a clean and smooth surface. They appear either on the casting surface or in the body of a casting.

These defects are caused by: 

  1. Excessive moisture content
  2. Inadequate gas permeability of the moulding sand
  3. Low pouring temperature

Shrinkage:

  • Volumetric contraction both in a solid and liquid state. Shrinkage due to thermal contraction of a liquid convert to solid-state.

Porosity or Permeability:

  • Permeability or porosity of the moulding sand is the measure of its ability to permit air to flow through it. Gases evolving from the molten metal and generated from the mould may have to go through the core to escape out of the mould. Hence cores are required to have higher permeability.

Inclusions:

  • Particles of slag, refractory materials, sand, or deoxidation products are trapped in the casting during pouring upon solidification. The provision of choke in the gating system and the pouring basin at the top of the mould can prevent this defect.

Latest MP Vyapam Sub Engineer Updates

Last updated on Dec 5, 2024

-> MP Vyapam Sub Engineer Recruitment 2024 Result has been declared for the exam which was held from 19th September 2024 onwards. 

-> A total of 283 vacancies have been announced. Candidates had applied online from 5th to 19th August 2024.

-> The MP Vyapam Sub Engineer exam aims to recruit individuals for Sub Engineer positions across various government departments in Madhya Pradesh.

-> Candidates can check MP Vyapam Sub Engineer Previous Year Papers for better preparation!

Hot Links: teen patti joy teen patti all games teen patti yas teen patti gold apk download